Preparation of hydroxyapatite from biological phosphorus
-
-
Abstract
Hydroxyapatite was prepared using biogenic phytic acid as phosphorus precursor and calcium hydroxide as calcium precursor.Hydroxyapatite was prepared by solid-liquid mixed ball milling combined with calcination.Optimum calcination temperature was 1 100 ℃, ball milling time was 2 h.Hydroxyapatite so prepared yielded high purity, and is a potential substitute for existing commercial supplies.
-
-